Originální abstrakt
The paper reports mechanical properties of magnesium alloy AZ31 deformed at low and high srain rates. Material was prepared using squeeze casting technology. Compresion test were deformed at an initial strain rate of 0,000083 1/s at temperatures between room temperature and 300 grad.Celsius. Dynamic compression Hopkinson test were carried out at room temperature with impact velocities ranging from 11,2 to 21,9 m/s. Transmission electron microscopy investigations showed significant dislocation and twins densities. Results are discussed considering the importance of the activation volume determined in the stress relaxation tests obtained at the low strain rate and quite separately, the importance of adiabatic shear banding at hihg strain rates.
Český abstrakt
Článek uvádí mechanické vlastnosti hořčíkové slitiny AZ31 deformované při nízkých a vysokých rychlostech deformace. Materiál byl připraven technologií lití. Kompresním testem byly vzorky deformovány při počáteční rychlosti deformace 0,000083 1 / s při teplotách mezi teplotou místnosti a 300 stupni Celsia. Kompresní dynamický Hopkinsonův test byl uskutečněn při teplotě místnosti a dopadové rychlosti impaktoru v rozmezí od 11,2 do 21,9 m / s. Transmisní elektronová mikroskopie ukázala významné hustoty dislokaci a dvojčata. Výsledky jsou diskutovány s ohledem na důležitost objemu aktivace stanovené v zátěžových relaxačních zkouškách získaných při nízké rychlosti deformace, a zcela samostatně, význam adiabatických smykových pásů při vysokých rychlostech deformace.
Anglický abstrakt
The paper reports mechanical properties of magnesium alloy AZ31 deformed at low and high srain rates. Material was prepared using squeeze casting technology. Compresion test were deformed at an initial strain rate of 0,000083 1/s at temperatures between room temperature and 300 grad.Celsius. Dynamic compression Hopkinson test were carried out at room temperature with impact velocities ranging from 11,2 to 21,9 m/s. Transmission electron microscopy investigations showed significant dislocation and twins densities. Results are discussed considering the importance of the activation volume determined in the stress relaxation tests obtained at the low strain rate and quite separately, the importance of adiabatic shear banding at hihg strain rates.
Klíčová slova česky
Hořčíkové slitiny; plasticita krystalu; zkouška tlakem; dislokace; dvojčatění;
Klíčová slova anglicky
Magnesium alloy; Crystal plasticity; Compression test; Dislocations; Twinning
Rok RIV
2013
Vydáno
12.03.2013
Nakladatel
Carl Hanser Verlag GmbH & Co.KG
Místo
München
ISSN
1862-5282
Ročník
2013
Číslo
104
Strany od–do
762–768
Počet stran
7
BIBTEX
@article{BUT107032,
author="Zuzanka {Trojanová} and Tomáš {Podrábský} and Pavel {Lukáč} and Ronald W {Armstrong} and Josef {Pešička} and Milan {Forejt},
title="Influence of strain rate on deformation mechanisms of an AZ31 magnesium alloy",
year="2013",
volume="2013",
number="104",
month="March",
pages="762--768",
publisher="Carl Hanser Verlag GmbH & Co.KG",
address="München",
issn="1862-5282"
}