Detail publikace

Zhutňování a slinování objemové ZrO2 a CeO2 nanokeramiky

TRUNEC, M. MACA, K. DOBŠÁK, P.

Český název

Zhutňování a slinování objemové ZrO2 a CeO2 nanokeramiky

Anglický název

Compaction and sintering of bulk zirconia and ceria nanoceramics

Typ

článek ve sborníku ve WoS nebo Scopus

Jazyk

en

Originální abstrakt

Shaping and sintering of bulk nanoceramic bodies were investigated. The results have shown that both shaping techniques, cold isostatic pressing and centrifugation, can be used to prepare almost fully dense (~99% of theoretical density) ceramic bodies provided the nanopowders are only weakly agglomerated and/or are properly dispersed through colloidal processing. Samples sintered at a temperature of 1500 degC did not display any nanocrystalline feature, the grain size ranged from 300 to 400 nm. Relative densities of 95.2% t.d. and 97.9% t.d. were achieved for selected ZrO2 bodies sintered at a temperature of 1100 degC for 4 hours and 1200 degC for 1 hour, respectively. At this temperature a nanocrystalline structure in sintered bodies was retained. The average grain size was 53 and 62 nm for a body sintered at 1100 degC and 1200 degC, respectively.

Český abstrakt

Bylo zkoumáno tvarování a slinování objemových nanokeramických těles. Výsledky ukázaly, že obě tvarovací techniky, isostatické lisování za studena a odstřeďování, mohly být použity pro přípravu téměř hutných (~99% teoretické hustoty) keramických těles, pokud nanoprášky byly pouze slabě aglomerované a/nebo byly vhodně dispergovány koloidními postupy. Vzorky slinované při 1500 degC neměly nanokrystalickou strukturu, velikost zrn se pohybovala od 300 do 400 nm. Relativní hustota 95,2% t.h. a 97,9% t.h. byla dosažena u vybraných ZrO2 těles slinovaných při 1100 degC po dobu 4 h a při 1200 degC po dobu 1 h. Při této slinovací teplotě byla nanokrystalická struktura zachována. Průměrná velikost zrn byla 53 a 62 nm pro tělesa slinovaná při 1100, resp. 1200 degC.

Anglický abstrakt

Shaping and sintering of bulk nanoceramic bodies were investigated. The results have shown that both shaping techniques, cold isostatic pressing and centrifugation, can be used to prepare almost fully dense (~99% of theoretical density) ceramic bodies provided the nanopowders are only weakly agglomerated and/or are properly dispersed through colloidal processing. Samples sintered at a temperature of 1500 degC did not display any nanocrystalline feature, the grain size ranged from 300 to 400 nm. Relative densities of 95.2% t.d. and 97.9% t.d. were achieved for selected ZrO2 bodies sintered at a temperature of 1100 degC for 4 hours and 1200 degC for 1 hour, respectively. At this temperature a nanocrystalline structure in sintered bodies was retained. The average grain size was 53 and 62 nm for a body sintered at 1100 degC and 1200 degC, respectively.

Klíčová slova anglicky

compaction, sintering, nanoceramics

Rok RIV

2003

Vydáno

01.01.2003

Nakladatel

International Community for Composuites Engineering

Místo

New Orleans

Kniha

Tenth annual international conference on composites/nano engineering

Číslo edice

1

Počet stran

2

BIBTEX


@inproceedings{BUT13311,
  author="Martin {Trunec} and Karel {Maca} and Petr {Dobšák},
  title="Compaction and sintering of bulk zirconia and ceria nanoceramics",
  booktitle="Tenth annual international conference on composites/nano engineering",
  year="2003",
  month="January",
  publisher="International Community for Composuites Engineering",
  address="New Orleans"
}